It Can Efficiently Manufacture Complex Precision Parts. Due To Its High Hardness And High Processing Difficulty, Traditional Processes Often Require Multiple Cutting Or Precision Casting, Which Is Costly And Limited In Design. The MIM Process Can Not Only Retain The High Temperature And Corrosion Resistance Of The Material, But Also Realize Complex Structures Such As Thin Walls And Small Holes, Such As Turbine Blades And Other Parts, While Reducing Material Waste, Which Is Suitable For Batch Production Of Small And Medium-Sized Parts.
Nickel-Based Alloys Need To Be Precisely Controlled During Degreasing And Sintering To Avoid Cracking Or Deformation. The Density And Mechanical Properties Of The Finished Product Are Close To The Traditional Forging Level.
Lead Time: < 15 Days
Tolerances: ±0.3% ~ ±0.5%
Max Part Size: Please Contact Us.
Available Superalloys at Dazao: Inconel 625, Inconel 718, Hastelloy X etc.
Inconel 625
Excellent Corrosion Resistance And Fatigue Performance, Suitable For Marine Environments And Chemical Equipment.
Superalloys Inconel 625 Properties
|
Tensile Strength, Yield (MPa) |
Fatigue Strength (MPa) |
Elongation at Break (%) |
Hardness (Brinell) |
Density (g/cm³) |
|
400-850 |
250-350 |
20-35 |
180-220 |
8.3-8.5 |
Inconel 718
A High-Strength Nickel-Chromium Alloy That Is Resistant To High-Temperature Oxidation And Creep. It Is Widely Used In Aerospace Engine Components (Such As Turbine Blades, Fuel Nozzles) And Aerospace Fasteners.
Superalloys Inconel 718 Properties
|
Tensile Strength, Yield (MPa) |
Fatigue Strength (MPa) |
Elongation at Break (%) |
Hardness (Brinell) |
Density (g/cm³) |
|
800-1300 |
300-500 |
10-20 |
300-380 |
8-8.1 |
Hastelloy X
Resistant To High-Temperature Oxidation And Hot Corrosion, Used For Gas Turbine Combustion Chamber Components.
Superalloys Hastelloy X Properties
|
Tensile Strength, Yield (MPa) |
Fatigue Strength (MPa) |
Elongation at Break (%) |
Hardness (Brinell) |
Density (g/cm³) |
|
400-800 |
250-350 |
30-40 |
180-220 |